MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik SAF 2507 Bar Steel
Categories: Metal; Ferrous Metal; Austenitic; Ferritic; Stainless Steel

Material Notes: Sandvik SAF 2507 is a high alloy duplex (austenitic-ferritic) stainless steel for service in highly corrosive conditions. It is characterized by:
  • excellent resistance to stress corrosion cracking in chloride bearing environments
  • excellent resistance to pitting and crevice corrosion
  • high resistance to general corrosion
  • very high mechanical strength
  • physical properties that offer design advantages
  • high resistance to erosion corrosion and corrosion fatigue good weldability
  • Information provided by Sandvik

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 7.80 g/cc0.282 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Brinell 260260
    Tensile Strength, Ultimate 760 - 930 MPa110000 - 135000 psi
    Tensile Strength, Yield >= 550 MPa
    @Strain 0.2 %
    >= 79800 psi
    @Strain 0.2 %
    Elongation at Break >= 25 %>= 25 %
    Modulus of Elasticity 200 GPa29000 ksi
     180 GPa
    @Temperature 300 °C
    26100 ksi
    @Temperature 572 °F
     186 GPa
    @Temperature 200 °C
    27000 ksi
    @Temperature 392 °F
     194 GPa
    @Temperature 100 °C
    28100 ksi
    @Temperature 212 °F
    Charpy Impact  150 J
    @Thickness 200 mm,
    Temperature -20.0 °C
    111 ft-lb
    @Thickness 7.87 in,
    Temperature -4.00 °F
     235 J
    @Thickness 85.0 mm,
    Temperature -20.0 °C
    173 ft-lb
    @Thickness 3.35 in,
    Temperature -4.00 °F
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  13.5 µm/m-°C
    @Temperature 30.0 - 100 °C
    7.50 µin/in-°F
    @Temperature 86.0 - 212 °F
     13.5 µm/m-°C
    @Temperature 30.0 - 100 °C
    7.50 µin/in-°F
    @Temperature 86.0 - 212 °F
     14.0 µm/m-°C
    @Temperature 30.0 - 200 °C
    7.78 µin/in-°F
    @Temperature 86.0 - 392 °F
     14.0 µm/m-°C
    @Temperature 30.0 - 300 °C
    7.78 µin/in-°F
    @Temperature 86.0 - 572 °F
     14.5 µm/m-°C
    @Temperature 30.0 - 400 °C
    8.06 µin/in-°F
    @Temperature 86.0 - 752 °F
    Specific Heat Capacity 0.490 J/g-°C0.117 BTU/lb-°F
     0.505 J/g-°C
    @Temperature 100 °C
    0.121 BTU/lb-°F
    @Temperature 212 °F
     0.520 J/g-°C
    @Temperature 200 °C
    0.124 BTU/lb-°F
    @Temperature 392 °F
     0.550 J/g-°C
    @Temperature 300 °C
    0.131 BTU/lb-°F
    @Temperature 572 °F
     0.585 J/g-°C
    @Temperature 400 °C
    0.140 BTU/lb-°F
    @Temperature 752 °F
    Thermal Conductivity 14.0 W/m-K97.2 BTU-in/hr-ft²-°F
     15.0 W/m-K
    @Temperature 100 °C
    104 BTU-in/hr-ft²-°F
    @Temperature 212 °F
     17.0 W/m-K
    @Temperature 200 °C
    118 BTU-in/hr-ft²-°F
    @Temperature 392 °F
     18.0 W/m-K
    @Temperature 300 °C
    125 BTU-in/hr-ft²-°F
    @Temperature 572 °F
     20.0 W/m-K
    @Temperature 400 °C
    139 BTU-in/hr-ft²-°F
    @Temperature 752 °F
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C <= 0.030 %<= 0.030 %
    Chromium, Cr 25 %25 %
    Copper, Cu <= 0.50 %<= 0.50 %
    Iron, Fe 61.1 %61.1 %As Balance
    Manganese, Mn <= 1.2 %<= 1.2 %
    Molybdenum, Mo 4.0 %4.0 %
    Nickel, Ni 7.0 %7.0 %
    Nitrogen, N 0.30 %0.30 %
    Phosphorus, P <= 0.035 %<= 0.035 %
    Silicon, Si <= 0.80 %<= 0.80 %
    Sulfur, S <= 0.015 %<= 0.015 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    316 Stainless Steel, annealed bar
    Sandvik SANMAC SAF 2205 Bar Steel
    MetalTek MTEK 2507 Cast UNS J93404 Duplex Stainless Steel
    Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
    Sandvik SAF 2507 Billet

    NSANDV140 / 19034

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.