MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik SAF 2507 Bar Steel
Categories: Metal; Ferrous Metal; Austenitic; Ferritic; Stainless Steel

Material Notes: Sandvik SAF 2507 is a high alloy duplex (austenitic-ferritic) stainless steel for service in highly corrosive conditions. It is characterized by:
  • excellent resistance to stress corrosion cracking in chloride bearing environments
  • excellent resistance to pitting and crevice corrosion
  • high resistance to general corrosion
  • very high mechanical strength
  • physical properties that offer design advantages
  • high resistance to erosion corrosion and corrosion fatigue good weldability
  • Information provided by Sandvik

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 7.80 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Brinell 260
    Tensile Strength, Ultimate 760 - 930 MPa
    Tensile Strength, Yield >= 550 MPa
    @Strain 0.2 %
    Elongation at Break >= 25 %
    Modulus of Elasticity 200 GPa
     180 GPa
    @Temperature 300 °C
     186 GPa
    @Temperature 200 °C
     194 GPa
    @Temperature 100 °C
    Charpy Impact 150 J
    @Thickness 200 mm,
    Temperature -20.0 °C
     235 J
    @Thickness 85.0 mm,
    Temperature -20.0 °C
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 13.5 µm/m-°C
    @Temperature 30.0 - 100 °C
     13.5 µm/m-°C
    @Temperature 30.0 - 100 °C
     14.0 µm/m-°C
    @Temperature 30.0 - 200 °C
     14.0 µm/m-°C
    @Temperature 30.0 - 300 °C
     14.5 µm/m-°C
    @Temperature 30.0 - 400 °C
    Specific Heat Capacity 0.490 J/g-°C
     0.505 J/g-°C
    @Temperature 100 °C
     0.520 J/g-°C
    @Temperature 200 °C
     0.550 J/g-°C
    @Temperature 300 °C
     0.585 J/g-°C
    @Temperature 400 °C
    Thermal Conductivity 14.0 W/m-K
     15.0 W/m-K
    @Temperature 100 °C
     17.0 W/m-K
    @Temperature 200 °C
     18.0 W/m-K
    @Temperature 300 °C
     20.0 W/m-K
    @Temperature 400 °C
     
    Component Elements PropertiesOriginal ValueComments
    Carbon, C <= 0.030 %
    Chromium, Cr 25 %
    Copper, Cu <= 0.50 %
    Iron, Fe 61.1 %As Balance
    Manganese, Mn <= 1.2 %
    Molybdenum, Mo 4.0 %
    Nickel, Ni 7.0 %
    Nitrogen, N 0.30 %
    Phosphorus, P <= 0.035 %
    Silicon, Si <= 0.80 %
    Sulfur, S <= 0.015 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    316 Stainless Steel, annealed bar
    Sandvik SANMAC SAF 2205 Bar Steel
    MetalTek MTEK 2507 Cast UNS J93404 Duplex Stainless Steel
    Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
    Sandvik SAF 2507 Billet

    NSANDV140 / 19034

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.