MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Sandvik SANMAC SAF 2205 Bar Steel
Categories: Metal; Ferrous Metal; Austenitic; Duplex; Ferritic; Stainless Steel

Material Notes: Sandvik SANMAC SAF 2205™ is a duplex stainless steel (austenitic-ferritic). It is characterized by:
  • high resistance to stress corrosion cracking in chloride-bearing environments
  • high resistance to stress corrosion cracking in environments containing hydrogen sulphide
  • high resistance to general corrosion, pitting and crevice corrosion
  • high mechanical strength – roughly twice the proof strength of austenitic stainless steels excellent machinability
  • good hot-working properties
  • high resistance to erosion corrosion and corrosion fatigue
  • physical properties that offer design advantages
  • good weldability
  • Information provided by Sandvik

    ASTM A479, A276; EN 1.4462; UNS S31803, S32205

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 7.80 g/cc0.282 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Brinell <= 270<= 270
    Tensile Strength, Ultimate 660 - 860 MPa95700 - 125000 psi
    Tensile Strength, Yield  >= 450 MPa
    @Strain 0.2 %
    >= 65300 psi
    @Strain 0.2 %
     >= 500 MPa
    @Strain 1 %
    >= 72500 psi
    @Strain 1 %
     >= 300 MPa
    @Strain 0.2 %,
    Temperature 250 °C
    >= 43500 psi
    @Strain 0.2 %,
    Temperature 482 °F
     >= 360 MPa
    @Strain 0.2 %,
    Temperature 100 °C
    >= 52200 psi
    @Strain 0.2 %,
    Temperature 212 °F
    Elongation at Break >= 25 %>= 25 %
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear 13.0 µm/m-°C
    @Temperature 30.0 - 100 °C
    7.22 µin/in-°F
    @Temperature 86.0 - 212 °F
    Specific Heat Capacity 0.480 J/g-°C
    @Temperature 20.0 °C
    0.115 BTU/lb-°F
    @Temperature 68.0 °F
    Thermal Conductivity 14.0 W/m-K
    @Temperature 20.0 °C
    97.2 BTU-in/hr-ft²-°F
    @Temperature 68.0 °F
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C <= 0.030 %<= 0.030 %
    Chromium, Cr 22.5 %22.5 %
    Iron, Fe 65.5 %65.5 %As Balance
    Manganese, Mn <= 2.0 %<= 2.0 %
    Molybdenum, Mo 3.2 %3.2 %
    Nickel, Ni 5.5 %5.5 %
    Nitrogen, N 0.18 %0.18 %
    Phosphorus, P <= 0.030 %<= 0.030 %
    Silicon, Si <= 1.0 %<= 1.0 %
    Sulfur, S <= 0.015 %<= 0.015 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Carlson 2205 (UNS S32205) Duplex Stainless Steel
    Sandvik SAF 2205 Billet
    Carlson 2205 (UNS S31803) Duplex Stainless Steel
    Outokumpu 2205 Duplex Stainless Steel
    AK Steel 2205 Duplex Stainless steel

    NSANDV146 / 19040

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.