Physical Properties | Metric | English | Comments |
---|
Density | 5.20 g/cc | 0.188 lb/in³ |
|
Chemical Properties | Metric | English | Comments |
---|
Acid Class, SR | 51.3 | 51.3 |
Alkali Class, AR | 2.3 | 2.3 |
Stain Resistance Class, FR | 3.0 | 3.0 |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Knoop | 360 | 360 |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 7.80 µm/m-°C @Temperature -30.0 - 70.0 °C | 4.33 µin/in-°F @Temperature -22.0 - 158 °F |
Transformation Temperature, Tg | 427 °C | 801 °F |
Softening Point | 529 °C | 984 °F |
|
Optical Properties | Metric | English | Comments |
---|
Refractive Index | 1.756 @Wavelength 2325.4 nm | 1.756 @Wavelength 2325.4 nm |
| 1.761 @Wavelength 1970.1 nm | 1.761 @Wavelength 1970.1 nm |
| 1.767 @Wavelength 1529.6 nm | 1.767 @Wavelength 1529.6 nm |
| 1.777 @Wavelength 1060 nm | 1.777 @Wavelength 1060 nm |
| 1.778 @Wavelength 1014 nm | 1.778 @Wavelength 1014 nm |
| 1.785 @Wavelength 852.1 nm | 1.785 @Wavelength 852.1 nm |
| 1.794 @Wavelength 706.5 nm | 1.794 @Wavelength 706.5 nm |
| 1.799 @Wavelength 656.3 nm | 1.799 @Wavelength 656.3 nm |
| 1.801 @Wavelength 643.8 nm | 1.801 @Wavelength 643.8 nm |
| 1.802 @Wavelength 632.8 nm | 1.802 @Wavelength 632.8 nm |
| 1.808 @Wavelength 589.3 nm | 1.808 @Wavelength 589.3 nm |
| 1.809 @Wavelength 587.6 nm | 1.809 @Wavelength 587.6 nm |
| 1.816 @Wavelength 546.1 nm | 1.816 @Wavelength 546.1 nm |
| 1.831 @Wavelength 486.1 nm | 1.831 @Wavelength 486.1 nm |
| 1.833 @Wavelength 480 nm | 1.833 @Wavelength 480 nm |
Abbe Number | 25.08 | 25.08 |
| 25.28 | 25.28 |
Optical Dispersion | 0.032015 | 0.032015 |
| 0.03257 | 0.03257 |
Transmission, Visible | 8.0 % @Thickness 25.0 mm, Wavelength 460 nm | 8.0 % @Thickness 0.984 in, Wavelength 460 nm |
| 9.0 % @Thickness 10.0 mm, Wavelength 460 nm | 9.0 % @Thickness 0.394 in, Wavelength 460 nm |
| 33 % @Thickness 25.0 mm, Wavelength 500 nm | 33 % @Thickness 0.984 in, Wavelength 500 nm |
| 64.2 % @Thickness 10.0 mm, Wavelength 500 nm | 64.2 % @Thickness 0.394 in, Wavelength 500 nm |
| 80.5 % @Thickness 25.0 mm, Wavelength 546 nm | 80.5 % @Thickness 0.984 in, Wavelength 546 nm |
| 89.8 % @Thickness 25.0 mm, Wavelength 580 nm | 89.8 % @Thickness 0.984 in, Wavelength 580 nm |
| 91.7 % @Thickness 10.0 mm, Wavelength 546 nm | 91.7 % @Thickness 0.394 in, Wavelength 546 nm |
| 93.1 % @Thickness 25.0 mm, Wavelength 620 nm | 93.1 % @Thickness 0.984 in, Wavelength 620 nm |
| 95 % @Thickness 25.0 mm, Wavelength 660 nm | 95 % @Thickness 0.984 in, Wavelength 660 nm |
| 95.8 % @Thickness 10.0 mm, Wavelength 580 nm | 95.8 % @Thickness 0.394 in, Wavelength 580 nm |
| 96.2 % @Thickness 25.0 mm, Wavelength 700 nm | 96.2 % @Thickness 0.984 in, Wavelength 700 nm |
| 97.2 % @Thickness 10.0 mm, Wavelength 620 nm | 97.2 % @Thickness 0.394 in, Wavelength 620 nm |
| 98 % @Thickness 10.0 mm, Wavelength 660 nm | 98 % @Thickness 0.394 in, Wavelength 660 nm |
| 98.5 % @Thickness 10.0 mm, Wavelength 700 nm | 98.5 % @Thickness 0.394 in, Wavelength 700 nm |
IR Transmittance | 66 % @Thickness 25.0 mm, Wavelength 2500 nm | 66 % @Thickness 0.984 in, Wavelength 2500 nm |
| 72.1 % @Thickness 25.0 mm, Wavelength 2325 nm | 72.1 % @Thickness 0.984 in, Wavelength 2325 nm |
| 84.4 % @Thickness 10.0 mm, Wavelength 2500 nm | 84.4 % @Thickness 0.394 in, Wavelength 2500 nm |
| 87.7 % @Thickness 10.0 mm, Wavelength 2325 nm | 87.7 % @Thickness 0.394 in, Wavelength 2325 nm |
| 91.5 % @Thickness 25.0 mm, Wavelength 1970 nm | 91.5 % @Thickness 0.984 in, Wavelength 1970 nm |
| 96.5 % @Thickness 10.0 mm, Wavelength 1970 nm | 96.5 % @Thickness 0.394 in, Wavelength 1970 nm |
| 98.7 % @Thickness 25.0 mm, Wavelength 1530 nm | 98.7 % @Thickness 0.984 in, Wavelength 1530 nm |
| 99.4 % @Thickness 25.0 mm, Wavelength 1060 nm | 99.4 % @Thickness 0.984 in, Wavelength 1060 nm |
| 99.5 % @Thickness 10.0 mm, Wavelength 1530 nm | 99.5 % @Thickness 0.394 in, Wavelength 1530 nm |
| 99.8 % @Thickness 10.0 mm, Wavelength 1060 nm | 99.8 % @Thickness 0.394 in, Wavelength 1060 nm |
|
Descriptive Properties |
---|
Climatic resistance | 4 |
Phosphate resistance | 3.3 |