MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott SF6G05 809253.520, Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes:

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.20 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 51.3
Alkali Class, AR 2.3
Stain Resistance Class, FR 3.0
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 360HK (0.1/20)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.80 µm/m-°C
@Temperature -30.0 - 70.0 °C
Transformation Temperature, Tg 427 °C
Softening Point 529 °Cviscosity of 107.6 cP
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.756
@Wavelength 2325.4 nm
 1.761
@Wavelength 1970.1 nm
 1.767
@Wavelength 1529.6 nm
 1.777
@Wavelength 1060 nm
 1.778
@Wavelength 1014 nm
 1.785
@Wavelength 852.1 nm
 1.794
@Wavelength 706.5 nm
 1.799
@Wavelength 656.3 nm
 1.801
@Wavelength 643.8 nm
 1.802
@Wavelength 632.8 nm
 1.808
@Wavelength 589.3 nm
 1.809
@Wavelength 587.6 nm
 1.816
@Wavelength 546.1 nm
 1.831
@Wavelength 486.1 nm
 1.833
@Wavelength 480 nm
Abbe Number 25.08ve
 25.28vd
Optical Dispersion 0.032015nf - nc
 0.03257nf' - nc'
Transmission, Visible 8.0 %
@Thickness 25.0 mm,
Wavelength 460 nm
 9.0 %
@Thickness 10.0 mm,
Wavelength 460 nm
 33 %
@Thickness 25.0 mm,
Wavelength 500 nm
 64.2 %
@Thickness 10.0 mm,
Wavelength 500 nm
 80.5 %
@Thickness 25.0 mm,
Wavelength 546 nm
 89.8 %
@Thickness 25.0 mm,
Wavelength 580 nm
 91.7 %
@Thickness 10.0 mm,
Wavelength 546 nm
 93.1 %
@Thickness 25.0 mm,
Wavelength 620 nm
 95 %
@Thickness 25.0 mm,
Wavelength 660 nm
 95.8 %
@Thickness 10.0 mm,
Wavelength 580 nm
 96.2 %
@Thickness 25.0 mm,
Wavelength 700 nm
 97.2 %
@Thickness 10.0 mm,
Wavelength 620 nm
 98 %
@Thickness 10.0 mm,
Wavelength 660 nm
 98.5 %
@Thickness 10.0 mm,
Wavelength 700 nm
IR Transmittance 66 %
@Thickness 25.0 mm,
Wavelength 2500 nm
 72.1 %
@Thickness 25.0 mm,
Wavelength 2325 nm
 84.4 %
@Thickness 10.0 mm,
Wavelength 2500 nm
 87.7 %
@Thickness 10.0 mm,
Wavelength 2325 nm
 91.5 %
@Thickness 25.0 mm,
Wavelength 1970 nm
 96.5 %
@Thickness 10.0 mm,
Wavelength 1970 nm
 98.7 %
@Thickness 25.0 mm,
Wavelength 1530 nm
 99.4 %
@Thickness 25.0 mm,
Wavelength 1060 nm
 99.5 %
@Thickness 10.0 mm,
Wavelength 1530 nm
 99.8 %
@Thickness 10.0 mm,
Wavelength 1060 nm
 
Descriptive Properties
Climatic resistance4
Phosphate resistance3.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott LAK9G15 691548.353, Optical Glass
DuPont Mobility and Materials Vespel® SP-1 ISO Polyimide
Schott N-LAK9 Glass
Schott ZERODUR® Glass Ceramic
Schott Sapphire Optical Window

CSGT9874 / 183127

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.