MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS Tristar® PC-10GF-HC 10% Glass Fiber Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: 10% Glass Fiber Reinforced Polycarbonate with Release. Non-Chlorine, Non Bromine FR system. Applications: Parts requiring High stiffness, close tolerances. Keywords: Non-Chlorine Non- Bromine Flame Retardant, UL 945VA, UL746H, RoHS.

Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Water Absorption 0.12 %
@Temperature 22.8 °C,
Time 86400 sec
0.12 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
@Thickness 3.17 mm
0.0020 - 0.0040 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 62.0 MPa
@Thickness 3.17 mm
8990 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 15 %
@Thickness 3.17 mm
15 %
@Thickness 0.125 in
ASTM D638
Flexural Strength 96.5 MPa
@Thickness 3.17 mm
14000 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 3.10 GPa
@Thickness 3.17 mm
450 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
Tensile Impact Strength 53.3 kJ/m²
@Thickness 3.17 mm
25.4 ft-lb/in²
@Thickness 0.125 in
ASTM D1822
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  3.00e+15 ohm-cm
@Treatment Temp. 90.0 °C,
Time 346000 sec
3.00e+15 ohm-cm
@Treatment Temp. 194 °F,
Time 96.0 hour
50% RH; ASTM D257
 6.00e+15 ohm-cm
@Treatment Temp. 23.0 °C,
Time 144000 sec
6.00e+15 ohm-cm
@Treatment Temp. 73.4 °F,
Time 40.0 hour
50% RH; ASTM D257
Dielectric Strength 19.0 kV/mm
@Thickness 3.00 mm
483 kV/in
@Thickness 0.118 in
ASTM D149
Arc Resistance 0.00 - 60 sec0.00 - 60 secPLC 7
Comparative Tracking Index 175 - 250 V175 - 250 VPLC 3
Hot Wire Ignition, HWI 30 - 60 sec30 - 60 secPLC 2
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsPLC 0
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min0.000 - 0.394 in/minPLC 0
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 138 °C280 °FASTM D648
UL RTI, Electrical 80.0 °C176 °F
 125 °C257 °F
UL RTI, Mechanical with Impact 80.0 °C176 °F
 115 °C239 °F
UL RTI, Mechanical without Impact 80.0 °C176 °F
 125 °C257 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
UL File # E155285
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 2.50 mm
V-0
@Thickness 0.0984 in
UL File # E155285
 5VA
@Thickness 2.50 mm
5VA
@Thickness 0.0984 in
UL File # E155285
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
UL File # E155285
Oxygen Index 37.1 %37.1 %ASTM D2863
Glow Wire Ignition Temperature 875 °C1610 °F
Glow Wire Flammability Index 960 °C1760 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 254 - 274 °C489 - 525 °F
Middle Barrel Temperature 266 - 277 °C511 - 531 °F
Front Barrel Temperature 277 - 293 °C531 - 559 °F
Nozzle Temperature 271 - 293 °C520 - 559 °F
Melt Temperature 282 - 304 °C540 - 579 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °Fsurface
Drying Temperature 121 °C
@Time 14400 sec
250 °F
@Time 4.00 hour
Injection Pressure 75.8 - 124 MPa11000 - 18000 psi
Back Pressure 0.345 - 1.38 MPa50.0 - 200 psi
Clamp Pressure 27.6 - 68.9 MPa4000 - 9990 psi
Shot Size 40 - 60 %40 - 60 %
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
Injection SpeedEdge Gate=slow to medium
 Tab Gate=medium to fast
 Tunnel Gate= fast
Non-Bromine, Non-Chlorinepass, UL 746H
Processing Methodinjection molding
RoHS CompliancePass, UL 746R

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Tristar® PC-10GF-HC-V 10% Glass Fiber Polycarbonate
Ashley Polymers Ashlene® 1021T Polycarbonate
Covestro Makrolon® 1260 Polycarbonate, Impact Grade
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow
Avient Edgetek® PC-10GF/000 Polycarbonate (PC), Glass Filled

PZ9PT93f / 198161

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.