MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Impact Modified

Material Notes: Polycarbonate, Impact Modified, Medium Flow

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 9.0 - 16 g/10 min
@Load 1.20 kg,
Temperature 300 °C
9.0 - 16 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 8989ASTM D785
Hardness, Rockwell R 121121ASTM D785
Tensile Strength at Break 53.8 MPa7800 psiASTM D638
Tensile Strength, Yield 51.7 MPa7500 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Flexural Strength 79.3 MPa11500 psiASTM D790
Flexural Modulus 2.07 GPa300 ksiASTM D790
Izod Impact, Notched  6.94 J/cm
@Temperature -17.8 °C
13.0 ft-lb/in
@Temperature 0.000 °F
ASTM D256
 8.01 J/cm
@Temperature 22.8 °C
15.0 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Gardner Impact 36.2 J26.7 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C255 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C245 °FASTM D648
Vicat Softening Point 141 °C285 °F120°C/h, 50 N; ASTM D1525
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0626 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 254 - 277 °C490 - 530 °F
Middle Barrel Temperature 266 - 288 °C510 - 550 °F
Front Barrel Temperature 277 - 299 °C530 - 570 °F
Melt Temperature 274 - 302 °C525 - 575 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 118 - 124 °C245 - 255 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.00127 cm0.000500 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Tristar® PC-10GF-HC 10% Glass Fiber Polycarbonate
Covestro Makrolon® 1260 Polycarbonate, Impact Grade
Ashley Polymers Ashlene® 1021T Polycarbonate

PPOLYQ178 / 160698

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.