10% Glass Fiber Reinforced Polycarbonate with Release. Non-Chlorine, Non Bromine FR system. Applications: Parts requiring High stiffness, close tolerances. Keywords: Non-Chlorine Non- Bromine Flame Retardant, UL 945VA, UL746H, RoHS.Information provided by Polymer Technology and Services, LLC (PTS). |