MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 4019, AE Condition
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 4000 Series Aluminum Alloy

Material Notes: Property data provided by RSP Technology.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 4019; AA4019; Al4019
Vendors: RSP Technology – Aluminum as strong as Titanium For more information contact: +31 (0)596 632 300 or visit www.rsp-technology.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.74 g/cc0.0990 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 140140
Tensile Strength, Ultimate 400 MPa58000 psi
 175 MPa
@Temperature 300 °C,
Time 3.60e+6 sec
25400 psi
@Temperature 572 °F,
Time 1000 hour
 250 MPa
@Temperature 250 °C,
Time 3.60e+6 sec
36300 psi
@Temperature 482 °F,
Time 1000 hour
 330 MPa
@Temperature 200 °C,
Time 3.60e+6 sec
47900 psi
@Temperature 392 °F,
Time 1000 hour
 380 MPa
@Temperature 150 °C,
Time 3.60e+6 sec
55100 psi
@Temperature 302 °F,
Time 1000 hour
 390 MPa
@Temperature 100 °C,
Time 3.60e+6 sec
56600 psi
@Temperature 212 °F,
Time 1000 hour
Tensile Strength, Yield 300 MPa43500 psi
 135 MPa
@Temperature 300 °C
19600 psi
@Temperature 572 °F
 180 MPa
@Temperature 250 °C
26100 psi
@Temperature 482 °F
 240 MPa
@Temperature 200 °C
34800 psi
@Temperature 392 °F
 280 MPa
@Temperature 150 °C
40600 psi
@Temperature 302 °F
 290 MPa
@Temperature 100 °C
42100 psi
@Temperature 212 °F
Elongation at Yield 2.5 %2.5 %
Tensile Modulus 90.0 GPa13100 ksi
Fatigue Strength 125 MPa
@Temperature 250 °C
18100 psi
@Temperature 482 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.30 µm/m-°C9.611 µin/in-°F
Thermal Conductivity 120 W/m-K833 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 70.7 - 75.1 %70.7 - 75.1 %As remainder
Iron, Fe 4.6 - 5.4 %4.6 - 5.4 %
Nickel, Ni 1.8 - 2.2 %1.8 - 2.2 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si 18.5 - 21.5 %18.5 - 21.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 4032-T6
Aluminum 4032-O
4015-H12 Aluminum
4015-O Aluminum
Aluminum 4043-H18

MA4019 / 9074

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.