MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 4019, AE Condition
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 4000 Series Aluminum Alloy

Material Notes: Property data provided by RSP Technology.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 4019; AA4019; Al4019
Vendors: RSP Technology – Aluminum as strong as Titanium For more information contact: +31 (0)596 632 300 or visit www.rsp-technology.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.74 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 140
Tensile Strength, Ultimate 400 MPa
 175 MPa
@Temperature 300 °C,
Time 3.60e+6 sec
 250 MPa
@Temperature 250 °C,
Time 3.60e+6 sec
 330 MPa
@Temperature 200 °C,
Time 3.60e+6 sec
 380 MPa
@Temperature 150 °C,
Time 3.60e+6 sec
 390 MPa
@Temperature 100 °C,
Time 3.60e+6 sec
Tensile Strength, Yield 300 MPa
 135 MPa
@Temperature 300 °C
 180 MPa
@Temperature 250 °C
 240 MPa
@Temperature 200 °C
 280 MPa
@Temperature 150 °C
 290 MPa
@Temperature 100 °C
Elongation at Yield 2.5 %
Tensile Modulus 90.0 GPa
Fatigue Strength 125 MPa
@Temperature 250 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.30 µm/m-°C
Thermal Conductivity 120 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 70.7 - 75.1 %As remainder
Iron, Fe 4.6 - 5.4 %
Nickel, Ni 1.8 - 2.2 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si 18.5 - 21.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 4032-T6
Aluminum 4032-O
4015-H12 Aluminum
4015-O Aluminum
Aluminum 4043-H18

MA4019 / 9074

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.