MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Product Description: EPO-TEK® OE188 is a low CTE, designed for semiconductor and fiber optic applications.

Advantages & Application Notes:

  • Paste-like viscosity allows for application by dispensing, or hand methods such as toothpick, spatula or pin transfer.
  • Color change upon cure – off-white to amber-brown - allows easy visual inspection.
  • The CTE value below the Tg keeps potential stress to a minimum.
  • Suggested applications:
    • Fiber Optic Packaging
      • Sealing fiber into the snout, ferrule, or feed-through of the opto-package.
      • Mounting optics, such as lenses, diodes, prisms, onto the substrate or “optical bench.”
      • Adhesive for building the optical bench to the correct Z-height.
      • “Toughened” adhesive to prevent fiber from the “piston effect”.
    • Semiconductor
      • As underfill of flip chip devices and SMDs like BGAs, capacitors and resistors.
    • Medical
      • As an alternative to EPO-TEK® 353ND for moisture resistance.
  • Capable of short cure cycles at low temperature, such as 80°C.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccPart B
 1.55 g/cc1.55 g/ccPart A
Particle Size <= 45 µm<= 45 µm
Viscosity 20000 - 30000 cP
@Temperature 23.0 °C
20000 - 30000 cP
@Temperature 73.4 °F
10 rpm
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) 9.0 ppm9.0 ppm
Ionic Impurities - Cl (Chloride) 188 ppm188 ppm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9191
Tensile Modulus 5.397 GPa782.8 ksiStorage
Shear Strength 10.92 MPa1584 psiLap
 >= 35.2 MPa>= 5100 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 7.00e+12 ohm-cm>= 7.00e+12 ohm-cm
Dielectric Constant 3.56
@Frequency 1000 Hz
3.56
@Frequency 1000 Hz
Dissipation Factor 0.0030
@Frequency 1000 Hz
0.0030
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.0 µm/m-°C10.6 µin/in-°FBelow Tg
 68.0 µm/m-°C37.8 µin/in-°FAbove Tg
Maximum Service Temperature, Air 225 °C437 °FContinuous
 325 °C617 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 90.0 °C>= 194 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 417 °C783 °FDegradation Temperature
 
Processing PropertiesMetricEnglishComments
Cure Time  1.00 min
@Temperature 150 °C
0.0167 hour
@Temperature 302 °F
minimum
 5.00 min
@Temperature 120 °C
0.0833 hour
@Temperature 248 °F
minimum
 10.0 min
@Temperature 100 °C
0.167 hour
@Temperature 212 °F
minimum
 30.0 min
@Temperature 80.0 °C
0.500 hour
@Temperature 176 °F
minimum
Pot Life 90 min90 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
ColorAmberPart B
 Off-WhitePart A
ConsistencySmooth paste
Ionic Impurities NH4304 ppm
Mix Ratio by Weight20:1
Number of ComponentsTwo
Thixotropic Index1.1
Weight Loss0.78%200°C
 1.9%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Anocast Silica-filled Epoxy Polymer Composite
Master Bond EP113 Two Component Epoxy
Master Bond EP112FLAO-1 Toughened, Two component, Heat Curing Epoxy
Master Bond EP121AO Thermally Conductive, Dimensionally Stable Epoxy System
Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive

PPOXYT143 / 141182

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.