MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 789-3 one component, high strength toughened adhesive is designed for microelectronic applications, including substrate attach and package sealing, which require good moisture resistance. It exhibits strong adhesion to difficult-to-bond metals, such as gold, silver and copper. This adhesive retains its bond strength after exposure to moisture. TRA-BOND 789-3 is available in a variety of colors to fit the application.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 36500 cP36500 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 37.9 MPa5500 psiLap shear, gold to gold
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm
Dielectric Constant 4.2
@Frequency 1000 Hz
4.2
@Frequency 1000 Hz
Dielectric Strength 31.5 kV/mm800 kV/in
Dissipation Factor 0.011
@Frequency 1000 Hz
0.011
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C35.0 µin/in-°FBelow Tg
 140 µm/m-°C77.8 µin/in-°FAbove Tg
Thermal Conductivity 0.300 W/m-K
@Temperature 121 °C
2.08 BTU-in/hr-ft²-°F
@Temperature 250 °F
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 126 °C259 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
 60.0 min
@Temperature 125 °C
1.00 hour
@Temperature 257 °F
Working Life 130000 min130000 min
Shelf Life 6.00 Month6.00 MonthAt 5°C
 12.0 Month
@Temperature -40.0 °C
12.0 Month
@Temperature -40.0 °F
 
Descriptive Properties
Color Cream
Outgassing, NASA Passes
Weight Loss % 0.28At 250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy
Permabond 737 Cyanoacrylate, toughened
Palm Labs Adhesives TURBO FUSE SERIES 180 BLACK TOUGHENED (2400 Viscosity) Rapid Bonding Adhesive
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive
Tra-Con Tra-Bond Ablebond 744-2NTN1 Electrically Insulating Polyimide Adhesive

PTRAC154 / 71082

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.