MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Glass Fiber Filled

Material Notes: Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige in color

Application Areas: Suitable for high temperature application, where higher strength needed in load-bearing application. Chemically resistant to aggressive environments, suitable for sterilization for medical and food contact applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/cc
Water Absorption 0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/in410°C nozzle, 220°C mold
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/in410°C nozzle, 220°C mold
Crystallinity 40 %40 %DSC
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 105105ASTM D785
Hardness, Shore D 9090
Tensile Strength at Break  50.0 MPa
@Temperature 250 °C
7250 psi
@Temperature 482 °F
ASTM D638
 65.0 MPa
@Temperature 200 °C
9430 psi
@Temperature 392 °F
ASTM D638
 100 MPa
@Temperature 150 °C
14500 psi
@Temperature 302 °F
ASTM D638
 135 MPa
@Temperature 100 °C
19600 psi
@Temperature 212 °F
ASTM D638
 185 MPa
@Temperature 23.0 °C
26800 psi
@Temperature 73.4 °F
ASTM D638
 190 MPa
@Temperature -10.0 °C
27600 psi
@Temperature 14.0 °F
ASTM D638
 205 MPa
@Temperature -50.0 °C
29700 psi
@Temperature -58.0 °F
ASTM D638
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %ASTM D638
Tensile Modulus 11.5 GPa1670 ksiASTM D638
Flexural Strength 280 MPa40600 psiASTM D790
Flexural Modulus 10.5 GPa1520 ksiASTM D790
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inASTM D256
Izod Impact, Unnotched 6.10 J/cm11.4 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistivity per Square 1.00e+16 ohm1.00e+16 ohmASTM D257
Dielectric Strength 14.0 kV/mm
@Thickness 3.20 mm
356 kV/in
@Thickness 0.126 in
ASTM D149
Arc Resistance 160 sec160 secat 500 Volts; ASTM D495
Comparative Tracking Index 140 V140 Vper 50 drops; ASTM D3638
 
Thermal PropertiesMetricEnglishComments
Melting Point 370 - 372 °C698 - 702 °FDSC
Deflection Temperature at 1.8 MPa (264 psi) 360 °C680 °F
Glass Transition Temp, Tg 152 - 154 °C306 - 309 °FDSC/onset
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 390 - 425 °C734 - 797 °F
Nozzle Temperature 425 °C797 °F
Mold Temperature 200 - 220 °C392 - 428 °F
Drying Temperature 150 °C302 °F
Dry Time 4 - 6 hour4 - 6 hour
 
Descriptive Properties
Hopper/ Throat Temperature60-80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gharda Chemicals G-PAEK™ 1200G Ultra High Performance PEK Polymer
Gharda Chemicals G-PAEK™ 1230CF Ultra High Performance PEK Polymer
Envalior Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber
Gharda Chemicals G-PAEK™ 1230FC Ultra High Performance PEK Polymer
Gharda Chemicals G-PAEK™ 1200P Ultra High Performance PEK Polymer

PGHARD995 / 108530

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.