MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik VESTAMID® NRG 4901 BK Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® NRG 4901 BK offers a flexible, mechanically tough encasement system that combines the advantages of polyethylene coating and cement mortar casing. Uses of VESTAMID® NRG products. The important advantages of VESTAMID® NRG 4901 as an encasement material are:
  • unusually high impact resistance and toughness, even at low temperatures
  • excellent stress cracking resistance
  • excellent wear resistance
  • low sliding friction coefficient
Product characteristics compared with other encasement materials. VESTAMID® NRG 4901 BK has higher Shore hardness than polyethylene or polypropylene. In contrast to polyethylene or propylene encasement, therefore, the polyamide encasement offers, apart from the corrosion protection provided by the barrier effect, also mechanical protection for the encased steel pipe. Application areas for the new encasement material are found in non-conventional installation technologies such as:
  • horizontal directional drilling
  • the soil displacement method with non-steered displacement hammers
  • dynamic ramming
  • plow technology
The manufacturer recommends a processing temperature between 230°C (446°F) and 260°C (500°F) – in some cases up to 280°C (536°F) - during the extrusion process. Preliminary data sheet.Therefore they must not be used to establish specifications. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Sustainable, Industry and Engineering, Energy, Oil and Gas
Sustainability: Sustainable electricity
Delivery form: Pellets, Granules
Additives: Unfilled
Applications: Corrosion protection, Encapsulation
Special Characteristics: High impact strength, Environmental stress crack resistance
Features: Low coefficient of friction
Color: Black

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Hardness, Shore D, ISO 7619-1
  • Ball Indentation Hardness, ISO 2039-1
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, ISO 527
  • Tensile Stress, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527, mat. nom. strain at br., etB
  • Elongation at Break, ISO 527, Nominal
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527
  • Charpy Impact Unnotched, ISO 179/1eU
  • Melting Point, ISO 11357-1/-3
  • Vicat Softening Point, ISO 306, 50 K/h
  • Melt Temperature, ISO 294, Injection Molding
  • Mold Temperature, ISO 294, Injection Molding
  • Injection Velocity, ISO 294, Injection Molding
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.