MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® NRG 4901 BK Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® NRG 4901 BK offers a flexible, mechanically tough encasement system that combines the advantages of polyethylene coating and cement mortar casing. Uses of VESTAMID® NRG products. The important advantages of VESTAMID® NRG 4901 as an encasement material are:
  • unusually high impact resistance and toughness, even at low temperatures
  • excellent stress cracking resistance
  • excellent wear resistance
  • low sliding friction coefficient
Product characteristics compared with other encasement materials. VESTAMID® NRG 4901 BK has higher Shore hardness than polyethylene or polypropylene. In contrast to polyethylene or propylene encasement, therefore, the polyamide encasement offers, apart from the corrosion protection provided by the barrier effect, also mechanical protection for the encased steel pipe. Application areas for the new encasement material are found in non-conventional installation technologies such as:
  • horizontal directional drilling
  • the soil displacement method with non-steered displacement hammers
  • dynamic ramming
  • plow technology
The manufacturer recommends a processing temperature between 230°C (446°F) and 260°C (500°F) – in some cases up to 280°C (536°F) - during the extrusion process. Preliminary data sheet.Therefore they must not be used to establish specifications. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Sustainable, Industry and Engineering, Energy, Oil and Gas
Sustainability: Sustainable electricity
Delivery form: Pellets, Granules
Additives: Unfilled
Applications: Corrosion protection, Encapsulation
Special Characteristics: High impact strength, Environmental stress crack resistance
Features: Low coefficient of friction
Color: Black

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 73.0
@Time 3.00 sec
ISO 7619-1
Ball Indentation Hardness 76.0 MPaISO 2039-1
Tensile Strength at Break 48.0 MPaISO 527
Tensile Strength 40.0 MPaISO 527
Tensile Stress 39.0 MPa
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 40.0 MPaISO 527
Elongation at Break >= 150 %mat. nom. strain at br., etB; ISO 527
 150 %Nominal; ISO 527
Elongation at Yield 12.0 %ISO 527
Tensile Modulus 1400 MPaISO 527
Charpy Impact Unnotched NB
@Temperature -40.0 °C
ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
Melting Point 177 °CISO 11357-1/-3
Vicat Softening Point 170 °C
@Load 1.02 kg
50 K/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection Molding; ISO 294
Mold Temperature 60.0 °CInjection Molding; ISO 294
Injection Velocity 200 mm/secInjection Molding; ISO 294
 
Descriptive Properties
Blue water consumption26.1 kgISO 14040, 14044
ColorBlack
Global Warming Potential2.7 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 5.8 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
 5.9 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7937 / 325069

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.