MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Quantum Composites
LyondellBasell Quantum AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC (As Cut)
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Composite SMC; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: AMC™ 8590 BK is a vinyl ester, chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat resistance and a low density. The carbon fiber is PAN based 12K tow.

  • Form = Sheet
  • Color = Black
  • Carbon Fiber Content = 53% nominal

Quantum Materials is now a part of LyondellBasell.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Specific Gravity
  • Linear Mold Shrinkage, ASTM D955
  • Linear Mold Shrinkage
  • Tensile Strength
  • Tensile Strength, ASTM D638
  • Tensile Modulus
  • Tensile Modulus, ASTM D638
  • Flexural Strength
  • Flexural Strength, ASTM D790
  • Flexural Modulus
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Poissons Ratio, ASTM D638
  • Shear Strength, Short Beam Shear
  • Maximum Service Temperature, Air, ASTM D648, Deflection Temperature, Load not specified
  • Glass Transition Temp, Tg, ASTM D4065
  • Glass Transition Temp, Tg
  • Processing Temperature, Compression Molding
  • Cure Time
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LYB Lyondell Basell, former Quantum Composites

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.