MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Quantum Composites AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Composite SMC; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: AMC™ 8590 BK is a vinyl ester, chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat resistance and a low density. The carbon fiber is PAN based 12K tow.

  • Form = Sheet
  • Color = Black
  • Carbon Fiber Content = 53% nominal

A. Schulman has acquired Quantum Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
Linear Mold Shrinkage <= 0.00 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 282 MPaASTM D638
Tensile Modulus 55.0 GPaASTM D638
Flexural Strength 606 MPaASTM D790
Flexural Modulus 38.5 GPaASTM D790
Compressive Strength 286 MPaASTM D695
Compressive Modulus 33.8 GPaASTM D695
Poissons Ratio 0.305ASTM D638
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 287 °CDeflection Temperature, Load not specified; ASTM D648
Glass Transition Temp, Tg 118 °CASTM D4065
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 310 °FCompression Molding
Cure Time 5.00 - 10.0 min
@Temperature 138 °C
Shelf Life 2.00 Month
@Temperature 23.9 °C
 
Descriptive Properties
Fiber Length (in)1Carbon, nominal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC
Quantum Composites AMC™ 8592 55% Carbon Fiber Reinforced SMC
Hexcel® HexMC® C / 2000 / R1 Composite SMC
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Quantum Composites AMC™ 2593 45% Carbon Fiber Reinforced Phenolic SMC

PCOQB906 / 139274

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.