MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Covestro Bayblend® MTR Extruded Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: Bayblend® MTR sheet is an opaque product offering a combination of low flammability characteristics, robust mechanical properties, and ease of fabrication. Bayblend MTR complies with the flammability and smoke emission requirements for transit materials per the U.S. Federal Railroad Administration, listed in DOT: 49 CFR 238, and meets the criteria in the Bombardier Transportation Standard SMP 800-C for Toxic Gas Generation. Bayblend MTR has lower specific gravity, higher stiffness, higher strength, and greater toughness than typical non-metallic materials used for mass transportation interior components. This combination of physical properties allows for design of thinner and lighter parts that often do not require secondary reinforcement or stiffeners. Bayblend MTR is available in a variety of textures and colors.

Applications: Thermoformed rail interior parts such as seating components, wall cladding, window reveals, and ceiling panels

Information provided by Covestro

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption at Equilibrium, ASTM D570
  • Hardness, Rockwell M, ASTM D785
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Modulus of Elasticity, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Impact Test, ASTM D3763
  • Volume Resistivity, ASTM D257
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear, ASTM D696
  • Thermal Conductivity, ASTM E1530
  • Insulation R Value, ASMT E1530, Btu-ft2-hr°F
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525
  • Smoke Density, ASTM D622, <100
  • Smoke Density, ASTM E622, <200
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.