Bayblend® MTR sheet is an opaque product offering a combination of low flammability characteristics, robust mechanical properties, and ease of fabrication. Bayblend MTR complies with the flammability and smoke emission requirements for transit materials per the U.S. Federal Railroad Administration, listed in DOT: 49 CFR 238, and meets the criteria in the Bombardier Transportation Standard SMP 800-C for Toxic Gas Generation. Bayblend MTR has lower specific gravity, higher stiffness, higher strength, and greater toughness than typical non-metallic materials used for mass transportation interior components. This combination of physical properties allows for design of thinner and lighter parts that often do not require secondary reinforcement or stiffeners. Bayblend MTR is available in a variety of textures and colors. Applications: Thermoformed rail interior parts such as seating components, wall cladding, window reveals, and ceiling panels Information provided by Covestro |