| KEBAFLEX / U D72 ST B.01 is a TPU with a Shore hardness of 72D. It is characterized by flexibility and good wear and abrasion resistance. Properties: flexible, good haptics, good gliding properties, good recovery behavior, High wear resistance, impact resistant Typical areas of application: Sealing elements, Spring elements, Sliding elements, Haptic components, industrial goods, Rollers, Gears, Timing belt Industries: Automotive, Household appliances, Industry, Agriculture, Mechanical Engineering, Sports & Recreation Information provided by BARLOG plastics GmbH. |