MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Barlog Plastics KEBAFLEX U D72 ST B.01 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: KEBAFLEX / U D72 ST B.01 is a TPU with a Shore hardness of 72D. It is characterized by flexibility and good wear and abrasion resistance.

Properties: flexible, good haptics, good gliding properties, good recovery behavior, High wear resistance, impact resistant

Typical areas of application: Sealing elements, Spring elements, Sliding elements, Haptic components, industrial goods, Rollers, Gears, Timing belt

Industries: Automotive, Household appliances, Industry, Agriculture, Mechanical Engineering, Sports & Recreation

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccISO 1183-1
Linear Mold Shrinkage, Flow 0.00600 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.00650 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72.0DIN ISO 7619-1
Tensile Strength at Break 49.0 MPaISO 527-1
Elongation at Break 345 %ISO 527-1
Charpy Impact Unnotched 100 kJ/m²ISO 179-1eU
Charpy Impact, Notched 100 kJ/m²ISO 179-1eA
Compression Set 42.0 %
@Treatment Temp. 23.0 °C
ISO 815-1
 63.0 %
@Treatment Temp. 70.0 °C
ISO 815-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 215 - 235 °C
Mold Temperature 20.0 - 50.0 °C
Drying Temperature 90.0 °C
Dry Time 2.00 - 3.00 hour
Moisture Content <= 0.0200 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBARLO583 / 326657

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.