MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
BYK Laponite® JS Clay Additive
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Laponite JS is a synthetic layered fluorosilicate modified with an inorganic polyphosphate dispersing agent. It hydrates and disperses in water to give virtually clear and colourless colloidal sols of low viscosity. At 18% concentration in water these sols will remain free flowing for at least 1 month.

Application: Laponite JS may be used in coating mixes to produce smooth, coherent, electrically conductive and anti-static films on paper, film and other surfaces. It may also be used in formulations to produce inkjet receiving coatings suitable for full colour printing. Films of Laponite JS demonstrate effective barrier properties by reducing migration of macromolecules and colloidal particles. Examples of binders suitable for use with Laponite JS include polyurethane, acrylic, vinyl acetate, SBR and polyvinyl alcohol.

Information provided by Southern Clay Products

Vendors:
Available Properties
  • Bulk Density
  • Particle Mesh Size, <2%
  • pH, 2% suspension
  • Specific Surface Area
  • Fluorine, F
  • H2O, Water, Free
  • Loss on Ignition(%)
  • MgO
  • Na2O
  • P2O5
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
former Southern Clay Products

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.