MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK Laponite® JS Clay Additive
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Laponite JS is a synthetic layered fluorosilicate modified with an inorganic polyphosphate dispersing agent. It hydrates and disperses in water to give virtually clear and colourless colloidal sols of low viscosity. At 18% concentration in water these sols will remain free flowing for at least 1 month.

Application: Laponite JS may be used in coating mixes to produce smooth, coherent, electrically conductive and anti-static films on paper, film and other surfaces. It may also be used in formulations to produce inkjet receiving coatings suitable for full colour printing. Films of Laponite JS demonstrate effective barrier properties by reducing migration of macromolecules and colloidal particles. Examples of binders suitable for use with Laponite JS include polyurethane, acrylic, vinyl acetate, SBR and polyvinyl alcohol.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 59.3 lb/ft³
Particle Mesh Size >= 250 Mesh<2%
pH 102% suspension
Specific Surface Area 300 m²/g
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 4.8 %
H2O, Water <= 10 %Free
Loss on Ignition(%) 8.7 %
MgO 22.2 %
Na2O 7.5 %
P2O5 5.4 %
SiO2 50.2 %
 
Descriptive Properties
Color/FormFree flowing white powder
Composition0.012Li2O

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Laponite® RDS Synthetic Layered Silicate
BYK Cloisite® 10A Nanoclay
BYK Laponite® SL25 Thickener
BYK Laponite® XLS Synthetic Layered Silicate
Dow TORAY Z-6265 SILANE

PBYK063 / 185060

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.