MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Hexcel® HexPly® F650 Bismaleimide Resin with Graphite F3T584 fabric reinforcement
Categories: Polymer; Thermoset; Bismaleimide (BMI)

Material Notes: Aging Data, (T300-3K, 8 H.S.); Laminate Physicals: 59.6% Fiber volume, 34.0% Resin content, 1.0% Voids

Information provided by HexCel

Key Words: BMI
Vendors:
Available Properties
  • Flexural Yield Strength, Control (Prepreg with no freezer or out time exposure)
  • Flexural Yield Strength, Phase V (Prepreg stored in freezer 1 year at -9°C and exposed to 60 days at RT)
  • Flexural Yield Strength, Phase I (Prepreg stored in freezer 4 months at -9°C and exposed to 30 days at RT)
  • Flexural Yield Strength, Phase II (Prepreg stored in freezer 4 months at -9°C and exposed to 60 days at RT)
  • Flexural Yield Strength, Phase III (Prepreg stored in freezer 6 months at -9°C and exposed to 60 days at RT)
  • Flexural Yield Strength, Phase IV (Prepreg stored in freezer 1 year at -9°C and exposed to 30 days at RT)
  • Flexural Yield Strength
  • Flexural Yield Strength
  • Flexural Yield Strength
  • Flexural Yield Strength
  • Flexural Yield Strength
  • Flexural Yield Strength
  • Compressive Yield Strength, Phase II (Prepreg stored in freezer 4 months at -9°C and exposed to 60 days at RT)
  • Compressive Yield Strength, Phase V (Prepreg stored in freezer 1 year at -9°C and exposed to 60 days at RT)
  • Compressive Yield Strength, Phase III (Prepreg stored in freezer 6 months at -9°C and exposed to 60 days at RT)
  • Compressive Yield Strength, Phase IV (Prepreg stored in freezer 1 year at -9°C and exposed to 30 days at RT)
  • Compressive Yield Strength, Phase I (Prepreg stored in freezer 4 months at -9°C and exposed to 30 days at RT)
  • Compressive Yield Strength, Control (Prepreg with no freezer or out time exposure)
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Shear Strength, Short Beam; Phase II (Prepreg stored in freezer 4 months at -9°C and exposed to 60 days at RT)
  • Shear Strength, Short Beam; Phase IV (Prepreg stored in freezer 1 year at -9°C and exposed to 30 days at RT)
  • Shear Strength, Short Beam; Phase I (Prepreg stored in freezer 4 months at -9°C and exposed to 30 days at RT)
  • Shear Strength, Short Beam; Phase V (Prepreg stored in freezer 1 year at -9°C and exposed to 60 days at RT)
  • Shear Strength
  • Shear Strength, Short Beam; Phase III (Prepreg stored in freezer 6 months at -9°C and exposed to 60 days at RT)
  • Shear Strength, Short Beam; Control (Prepreg with no freezer or out time exposure)
  • Shear Strength
  • Shear Strength
  • Shear Strength
  • Shear Strength
  • Shear Strength
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.