MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik VESTAKEEP® 4500 G PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® 4500 G is a high viscosity, fast cristallization, unreinforced polyether ether ketone for injection molding and extrusion. The semi-crystalline polymer features superior, thermal and chemical resistance. Parts made from VESTAKEEP® 4500 G are of low flammability. VESTAKEEP® 4500 G can be processed by common machines for thermoplastics. The manufacturer recommends a melt temperature between 370°C and 380°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C. VESTAKEEP® 4500 G is supplied as granules in 25kg boxes with moisture-proof polyethylene liners. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. Pigmentation may affect values
Dry properties listed below
Industrial Sector: Automotive and Mobility, Industry and Engineering, Energy, Oil and Gas
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Optics: Opaque
Resistance to: Heat (thermal stability), Fire / burn
Electrical: Insulating
Conformity: Food contact
Additives: Unfilled
Applications: General purpose
Processing: Profile extrusion, Sheet extrusion
Special Characteristics: Semi-crystalline, High viscosity
Color: Natural color
Chemical Resistance: General chemical resistance

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Viscosity, Melt
  • Linear Mold Shrinkage, Flow, ISO 294-4, 2577
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 2577
  • Melt Flow, ISO 1133
  • Hardness, Shore D, ISO 7619-1
  • Tensile Strength, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527, Nominal
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Volume Resistivity, IEC 62631-3-1, ?V
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Strength, IEC 60243-1, AC, S20/P25
  • Dielectric Strength, IEC 60243-1, AC, P25/P25
  • Dielectric Strength, ASTM D149, Short Time
  • Dielectric Strength, IEC 60243-1, AC, S20/S20, t
  • Dissipation Factor, IEC 62631-2-1
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2
  • Melting Point, ISO 11357-1/-3
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Glass Transition Temp, Tg, ISO 11357
  • Flammability, UL94, IEC 60695-11-10
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Feed Temperature, Injection Molding
  • Feed Temperature, Plastification
  • Zone 1, Plastification
  • Zone 2, Plastification
  • Zone 3, Plastification
  • Zone 4, Plastification
  • Zone 5, Plastification
  • Melt Temperature
  • Melt Temperature, ISO 294, Injection Molding
  • Melt Temperature, Plastification
  • Mold Temperature, ISO 294, Injection Molding
  • Mold Temperature
  • Drying Temperature, Pre-drying
  • Drying Temperature, Pre-drying, Pretreatment
  • Dry Time, Pre-drying
  • Dry Time, Pre-drying, Pretreatment
  • Moisture Content, processing humidity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.