MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
INEOS Styrolution Styrolux® T1 SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Product Description: Styrolux® T1 is a new, clear and tough styrene butadiene copolymer (SBC) designed specifically for high performance film extrusion and shrink film applications. Styrolux® T1 has been developed for blending with a second SBC component, Styrolux® S, which increases the stiffness of the film and improves the storage stability of film reels (reduced natural shrinkage).
Features: Excellent clarity and toughness; High shrinkage up to 70%; Very good shrinkage control; Low gel content; Reduced film stickiness
Applications: Blend component for Styrolux S; Shrink sleeve applications; Label film

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Block Copolymer; Good Toughness; High Clarity; High Shrinkage; Low Gel

Uses: Blending; Film; Labels; Shrink Wrap

Appearance: Clear/Transparent

Form: Pellets

Processing Method: Film Extrusion

Information provided by INEOS Styrolution

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption at Saturation, ISO 62
  • Melt Flow, ISO 1133
  • Melt Flow, ISO 1133
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Yield, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Tensile Modulus, ISO 527-1
  • Charpy Impact Unnotched, ISO 179/1eU
  • Volume Resistivity, IEC 62631-2-1
  • Surface Resistance, IEC 62631-3-1
  • Dissipation Factor, IEC 62631-2-1
  • Comparative Tracking Index, IEC 60112
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-2/B, Annealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Annealed
  • Vicat Softening Point, ISO 306/B50
  • Refractive Index, ISO 489, Sodium D Line
  • Haze, ASTM D1003
  • Transmission, Visible, ASTM D1003
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.