MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
INEOS Styrolution Styrolux® T1 SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Product Description: Styrolux® T1 is a new, clear and tough styrene butadiene copolymer (SBC) designed specifically for high performance film extrusion and shrink film applications. Styrolux® T1 has been developed for blending with a second SBC component, Styrolux® S, which increases the stiffness of the film and improves the storage stability of film reels (reduced natural shrinkage).
Features: Excellent clarity and toughness; High shrinkage up to 70%; Very good shrinkage control; Low gel content; Reduced film stickiness
Applications: Blend component for Styrolux S; Shrink sleeve applications; Label film

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Block Copolymer; Good Toughness; High Clarity; High Shrinkage; Low Gel

Uses: Blending; Film; Labels; Shrink Wrap

Appearance: Clear/Transparent

Form: Pellets

Processing Method: Film Extrusion

Information provided by INEOS Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Water Absorption at Saturation 0.070 %ISO 62
Melt Flow 12 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 75 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64ISO 868
Tensile Strength, Yield 3630 psiISO 527-2
Elongation at Break 250 %ISO 527-2
Tensile Modulus 160000 psiISO 527-1
Charpy Impact Unnotched >= 38.0 ft-lb/in²ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 62631-2-1
Surface Resistance 1.00e+15 ohmIEC 62631-3-1
Dissipation Factor 0.00030IEC 62631-2-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 131 °FAnnealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 122 °FAnnealed; ISO 75-2/A
Vicat Softening Point 118 °FISO 306/B50
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.57Sodium D Line; ISO 489
Haze 1.5 %ASTM D1003
Transmission, Visible 91 %
@Thickness 14000 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 356 - 446 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTYS773 / 311466

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.