MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Indium Corp. IndiSulâ„¢ In2(SO4)3 - 9H2O Indium Sulfate Hydrated Salt
Categories: Ceramic

Material Notes: Indium Sulfate is a grayish-white powder. It is hydroscopic and possesses a monoclinic prism structure. It is available as an anhydrous powder, a hydrated salt with 9 moles of associated water, and a solution in varying concentrations up to its solubility limit in water. Indium Sulfate is used as a synthesis chemical and as a hardening agent in gold electroplating baths.

Properties

  • Chemical Formula: In2(SO4)3 - 9H2O
  • General Description: Grayish white hydroscopic powder; monoclinic prisms
  • Purity Grades Available: 4N (99.99%), 5N (99.999%)

Uses

  • Chemical synthesis
  • Hardening agent in gold electroplating baths

Information Provided by Indium Corporation

Vendors:
Available Properties
  • Specific Gravity
  • Solubility in Water
  • Molecular Weight
  • Vapor Pressure, Dissociation Pressure
  • Vapor Pressure, Dissociation Pressure
  • Specific Heat Capacity
  • Indium, In
  • Indium, In, Theoretical
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Indium Corporation

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.