MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Indium Corp. IndiSul™ In2(SO4)3 - 9H2O Indium Sulfate Hydrated Salt
Categories: Ceramic

Material Notes: Indium Sulfate is a grayish-white powder. It is hydroscopic and possesses a monoclinic prism structure. It is available as an anhydrous powder, a hydrated salt with 9 moles of associated water, and a solution in varying concentrations up to its solubility limit in water. Indium Sulfate is used as a synthesis chemical and as a hardening agent in gold electroplating baths.

Properties

  • Chemical Formula: In2(SO4)3 - 9H2O
  • General Description: Grayish white hydroscopic powder; monoclinic prisms
  • Purity Grades Available: 4N (99.99%), 5N (99.999%)

Uses

  • Chemical synthesis
  • Hardening agent in gold electroplating baths

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.438 g/cc
Solubility in Water 53.92 %
@Temperature 20.0 °C
Molecular Weight 679.95 g/mol
Vapor Pressure 10.0 torr
@Temperature 645 °C
Dissociation Pressure
 900 torr
@Temperature 820 °C
Dissociation Pressure
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.540 J/g-°C
@Temperature 0.000 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Indium, In 31.5 - 35.9 %
 33.77 %Theoretical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sodium Chloride, NaCl (Halite)
MarkeTech Sodium Iodide:Thallium (Nal:Tl) Scintillator Crystal
Sodium Iodide, NaI
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal

NNIN937 / 131576

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.