MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Zircar Zirconia ZOF-100 Pure Zirconia Felt Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zircar’s unique process for manufacturing yttria-stabilized zirconia cloths and felts is also used in the production of pure zirconia refractory fibers and textiles without stabilizers. For those processes which are intolerant of yttria, these unstabilized pure zirconia fiber products provide much of the same high performance insulating benefits. Pure zirconia fibers exist in the monoclinic crystal phase and appear white in color. Our high purity zirconia fiber and textiles are offered in six different standard product forms; bulk fiber Type ZOBF, two felts Types ZOF-50 and ZOF-100 and three types of knit cloth Types ZOK-15, ZOW-15 and ZOW-30.

Features:

  • High Purity Zirconia
  • High Temperature Stability
  • Low Thermal Conductivity
  • Excellent Thermal Shock Resistance
  • No Outgassing
  • Six Different Product Formats Offered
  • Available ‘Off the Shelf’

Application Information:

  • Pure zirconia cloth is used as high temperature insulation for advanced energy systems.

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors:
Available Properties
  • Loss On Ignition
  • Outgassing - Total Mass Loss
  • Melting Point
  • Shrinkage
  • CaO
  • HfO2
  • Na2O
  • SiO2
  • Y2O3
  • ZrO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.