MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zircar Zirconia ZOF-100 Pure Zirconia Felt Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zircar’s unique process for manufacturing yttria-stabilized zirconia cloths and felts is also used in the production of pure zirconia refractory fibers and textiles without stabilizers. For those processes which are intolerant of yttria, these unstabilized pure zirconia fiber products provide much of the same high performance insulating benefits. Pure zirconia fibers exist in the monoclinic crystal phase and appear white in color. Our high purity zirconia fiber and textiles are offered in six different standard product forms; bulk fiber Type ZOBF, two felts Types ZOF-50 and ZOF-100 and three types of knit cloth Types ZOK-15, ZOW-15 and ZOW-30.

Features:

  • High Purity Zirconia
  • High Temperature Stability
  • Low Thermal Conductivity
  • Excellent Thermal Shock Resistance
  • No Outgassing
  • Six Different Product Formats Offered
  • Available ‘Off the Shelf’

Application Information:

  • Pure zirconia cloth is used as high temperature insulation for advanced energy systems.

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Loss On Ignition 0.34 %
@Temperature 950 °C,
Time 3600 sec
Outgassing - Total Mass Loss 0.00 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 2590 °C
Shrinkage 0.00 %
@Temperature 1650 °C,
Time 3600 sec
 
Component Elements PropertiesOriginal ValueComments
CaO 0.040 %
HfO2 1.0 - 2.0 %
Na2O 0.020 %
SiO2 0.22 %
Y2O3 <= 0.0010 %
ZrO2 >= 97 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, Alpha SiC
Yttria Stabilized Zirconia, YSZ
AISI Type A2 Tool Steel
PSM Industries Pacific Sintered Metals FX-227-T Infiltrated Steel Powdered Metal (MPIF FX-1005-50)
Sapco Silicon Nitride, Si3N4

C6ZIR034 / 2790

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.