MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Park Aerospace Nelco® N5000-30/32 BT Epoxy Package
Categories: Polymer; Thermoset; Epoxy

Material Notes: The Nelco N5000-30 prepreg and N5000-32 laminate BT epoxy materials are designed specifically to meet or exceed new and emerging chippackaging requirements. The primary applications of these materials include high performance interconnects that form the circuitry inside plastic BGAs, PBGAs and LGAs.

Key Features and Benefits:

  • BT resin chemistry
  • Excellent Reliability and Performance
  • Chip Packaging Options
  • Meets JEDEC Standards
  • Wide processing latitude

Applications/Qualifications:

  • BGA Multilayers
  • PBGA
  • LG
  • PCMCIA
  • MCM-Ls
  • Direct Chip Attach
  • JEDEC Conforming Packages
  • RoHS Compliant
  • Meets IPC-4101/30 Specifications

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors:
Available Properties
  • Water Absorption, IPC-TM-650.2.6.2.1
  • Modulus of Elasticity, ASTM D3039, Y
  • Modulus of Elasticity, ASTM D3039, X
  • Poissons Ratio, ASTM D3039, X
  • Poissons Ratio, ASTM D3039, Y
  • Shear Modulus, Calculated
  • Peel Strength, IPC-TM-650.2.4.8.2a, at elevated temperature
  • Peel Strength, IPC-TM-650.2.4.8, after solder float
  • Volume Resistivity, IPC-TM-650.2.5.17.1, C - 96/35/90
  • Surface Resistance, IPC-TM-650.2.5.17.1, C - 96/35/90
  • Dielectric Constant, IPC-TM-650.2.5.5.9, RF Impedance
  • Dielectric Constant, IPC-TM-650.2.5.5.3, TFC/LCR Meter
  • Dielectric Strength, IPC-TM-650.2.5.6.2
  • Dielectric Breakdown, IPC-TM-650.2.5.6
  • Dissipation Factor, IPC-TM-650.2.5.5.3, TFC/LCR Meter
  • Arc Resistance, IPC-TM-650.2.5.1
  • CTE, linear, IPC-TM-650.2.4.41
  • Glass Transition Temp, Tg, IPC-TM-650.2.4.24.3, DMA (Tan d Peak)
  • Decomposition Temperature, IPC-TM-650.2.4.24.6, 5% weight loss; TGA
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Park Aerospace, former Park Electrochemical Corp.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.