MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Syensqo (Solvay Specialty Polymers) Parmax® 1200 Self-Reinforcing Polyethersulfone  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: PARMAX 1200 self-reinforcing polymer (SRP) is an ultra-high performance amorphous, melt-processable engineering thermoplastic. The unique properties of this material are due primarily to the inherent rigid-rod structure. PARMAX SRP is differentiated from other thermoplastics by outstanding mechanical properties without fiber reinforcement, scratch resistance, great friction and wear properties, excellent solvent resistance, and exceptional low temperature performance.

PARMAX 1200 SRP has great thermal and thermal-oxidative stability and it is noncombustible. The specific strength of PARMAX 1200 SRP exceeds many of the materials commonly encountered in structural applications. The resin also possesses excellent machinability permitting fabrication of parts such as fasteners to tolerances of less than one mil (0.025 mm).

The excellent mechanical, chemical, thermal, and physical properties of PARMAX 1200 SRP make it the material of choice for a variety of applications including aircraft substructures, semiconductor components, bushings, bearings, and gears, light-weight vehicle suspensions systems, and medical tubing and other devices.

PARMAX 1200 resin comes in natural or black pellets as extrusion grade – PARMAX 1200 EP (NT-001 and BK-002) and as Krum for compression molding – PARMAX 1200 CK (NT-001 and BK-002).

Information provided by Solvay Advanced Polymers

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, ASTM D570, 24 hours
  • Moisture Absorption at Equilibrium, ASTM D570
  • Tensile Strength at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Yield Strength, ASTM D695
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Dielectric Constant, ASTM D150
  • CTE, linear, ASTM E 831
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Glass Transition Temp, Tg, ASTM E 1356
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.