MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Parmax® 1200 Self-Reinforcing Polyethersulfone  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: PARMAX 1200 self-reinforcing polymer (SRP) is an ultra-high performance amorphous, melt-processable engineering thermoplastic. The unique properties of this material are due primarily to the inherent rigid-rod structure. PARMAX SRP is differentiated from other thermoplastics by outstanding mechanical properties without fiber reinforcement, scratch resistance, great friction and wear properties, excellent solvent resistance, and exceptional low temperature performance.

PARMAX 1200 SRP has great thermal and thermal-oxidative stability and it is noncombustible. The specific strength of PARMAX 1200 SRP exceeds many of the materials commonly encountered in structural applications. The resin also possesses excellent machinability permitting fabrication of parts such as fasteners to tolerances of less than one mil (0.025 mm).

The excellent mechanical, chemical, thermal, and physical properties of PARMAX 1200 SRP make it the material of choice for a variety of applications including aircraft substructures, semiconductor components, bushings, bearings, and gears, light-weight vehicle suspensions systems, and medical tubing and other devices.

PARMAX 1200 resin comes in natural or black pellets as extrusion grade – PARMAX 1200 EP (NT-001 and BK-002) and as Krum for compression molding – PARMAX 1200 CK (NT-001 and BK-002).

Information provided by Solvay Advanced Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Moisture Absorption 0.20 %24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.70 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30000 psiASTM D638
Tensile Modulus 1.20e+6 psiASTM D638
Flexural Strength 45.0 ksiASTM D790
Flexural Modulus 1200 ksiASTM D790
Compressive Yield Strength 35.0 ksiASTM D695
Izod Impact, Notched 0.800 ft-lb/inASTM D256
Izod Impact, Unnotched 20.0 ft-lb/inASTM D4812
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.1
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µin/in-°F
@Temperature 20.0 °C
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 320 °FASTM D648
Glass Transition Temp, Tg 316 °FASTM E 1356
Flammability, UL94 V-0
@Thickness 0.254 mm
Oxygen Index 49 %ASTM D2863
 
Descriptive Properties
Pencil Hardness7HASTM D3363
Smoke Emission, DsMax 1 at 1.5 minASTM E662
 Max 1 at 4 minASTM E662

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) PrimoSpire® PR-9120 Self-reinforced Polyphenylene
Saint-Gobain Rulon® W2 Bearing/Seal PTFE
Ovation Polymers UTTAP SF 50030GF Polyethersulfone, 30% Glass Reinforced
BASF Ultrason® S 2010 G4 20% Glass Filled PSU

PSOL98 / 67937

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.