MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ChevronTexaco Delo® Synthetic Grease SF
Categories: Fluid; Lubricant; Polyalphaolefin (PAO); Urea Gellant

Material Notes: Features

Chevron Delo Synthetic Grease SF is a high performance grease specifically engineered for trailer wheel-ends operating in all conditions, even under the most extreme high and low temperatures, and for those demanding applications requiring extended lubrication intervals.

It is manufactured using polyalphaolefin (PAO) synthetic base oil, a polyurea thickener, rust and oxidation inhibitors, extreme pressure additives, and a special combination of friction reducing agents. It is gold in color with a smooth, semifluid texture. Chevron Delo Synthetic Grease SF is formulated to perform in unusually demanding conditions of high and low temperatures. The polyurea thickener in Chevron Delo Synthetic Grease SF elevates the dropping point to 250°C (482°F). This high dropping point equates to excellent high temperature stability up to 190°C (375°F). In addition, the high viscosity index (VI) of the PAO synthetic base oil allows for excellent flow properties at low temperatures - allowing Chevron Delo Synthetic Grease SF to operate at temperatures as low as -45°C (-50°F).

Applications

Trailer lubrication — Chevron Delo Synthetic Grease SF is recommended for use in trailer axles. It flows smoothly and evenly at temperatures as low as -46°C (-50°F) and continues to lubricate efficiently at temperatures up to 191°C (375°F). It provides many advantages in trailer axle lubrication, compared to mineral oil-based grease, such as

  • Excellent low temperature properties (i.e. lower starting torque).
  • Oxidation resistance at high temperatures.
  • Low incidence of seal leakage through use of a grease as compared with the conventional SAE 80W- 90 gear oil.
  • Excellent antiwear/low friction performance throughout the operating temperature range.

Industrial lubrication — Chevron Delo Synthetic Grease SF lubricates yearlong under the most severe operating conditions. Along with wide temperature range performance, Chevron Delo Synthetic Grease SF provides excellent industrial equipment lubrication with a special blend of additives, including organo-moly, to resist oxidation, protect against rust, enhance antiwear properties and ensure long lubricating life under conditions of extreme pressure and temperature. Field tests showed Chevron Delo Synthetic Grease SF to be particularly effective in industrial gear lubrication.

Key Words: CPS Number: 235253; MSDS Number: 7750
Vendors:
Available Properties
  • Viscosity Measurement, ASTM D2270, Viscosity Index of base oil
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Four Ball Extreme Pressure, Weld Load, Weld Point
  • Four Ball Wear
  • Penetration, Worked
  • Penetration P(0), 1/10 mm
  • Timken Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dropping Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.