MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco Delo® Synthetic Grease SF
Categories: Fluid; Lubricant; Polyalphaolefin (PAO); Urea Gellant

Material Notes: Features

Chevron Delo Synthetic Grease SF is a high performance grease specifically engineered for trailer wheel-ends operating in all conditions, even under the most extreme high and low temperatures, and for those demanding applications requiring extended lubrication intervals.

It is manufactured using polyalphaolefin (PAO) synthetic base oil, a polyurea thickener, rust and oxidation inhibitors, extreme pressure additives, and a special combination of friction reducing agents. It is gold in color with a smooth, semifluid texture. Chevron Delo Synthetic Grease SF is formulated to perform in unusually demanding conditions of high and low temperatures. The polyurea thickener in Chevron Delo Synthetic Grease SF elevates the dropping point to 250°C (482°F). This high dropping point equates to excellent high temperature stability up to 190°C (375°F). In addition, the high viscosity index (VI) of the PAO synthetic base oil allows for excellent flow properties at low temperatures - allowing Chevron Delo Synthetic Grease SF to operate at temperatures as low as -45°C (-50°F).

Applications

Trailer lubrication — Chevron Delo Synthetic Grease SF is recommended for use in trailer axles. It flows smoothly and evenly at temperatures as low as -46°C (-50°F) and continues to lubricate efficiently at temperatures up to 191°C (375°F). It provides many advantages in trailer axle lubrication, compared to mineral oil-based grease, such as

  • Excellent low temperature properties (i.e. lower starting torque).
  • Oxidation resistance at high temperatures.
  • Low incidence of seal leakage through use of a grease as compared with the conventional SAE 80W- 90 gear oil.
  • Excellent antiwear/low friction performance throughout the operating temperature range.

Industrial lubrication — Chevron Delo Synthetic Grease SF lubricates yearlong under the most severe operating conditions. Along with wide temperature range performance, Chevron Delo Synthetic Grease SF provides excellent industrial equipment lubrication with a special blend of additives, including organo-moly, to resist oxidation, protect against rust, enhance antiwear properties and ensure long lubricating life under conditions of extreme pressure and temperature. Field tests showed Chevron Delo Synthetic Grease SF to be particularly effective in industrial gear lubrication.

Key Words: CPS Number: 235253; MSDS Number: 7750
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 150Viscosity Index of base oil; ASTM D2270
Saybolt Viscosity at 100°F 637 SUS
Saybolt Viscosity at 210°F 88 SUS
Kinematic Viscosity at 40°C (104°F) 124 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 17 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 200 kgWeld Point
Four Ball Wear 0.340 mm
Penetration 380Worked
Penetration P(0), 1/10 mm 265
Timken Test 45.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 190 °C
Minimum Service Temperature, Air -45.0 °C
Dropping Point 230 °C
 
Descriptive Properties
Bearing RustPass
ColorGold
Low Temperature Running Torque, -40°F, Nm 0.9
Low Temperature Starting Torque, -40°F, Nm 1.4
TextureSmooth, Semifluid
Thickener, % / type9 / Polyurea
U.S. Steel Pumpability, -40°F, g/min at 150 psi13.3
U.S. Steel Pumpability, -40°F, g/min at 50 psi0.4
 7.7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives Thermoset™ TC-208 Thermally Conductive Grease
ExxonMobil Mobil Rarus 824
ExxonMobil Mobil Aero HFA
Dow HIGH VACUUM GREASE
ChevronTexaco TEGRA® Synthetic Barrier Fluid

WCHEV247 / 74862

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.