MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Borealis Borstar® FB2230 LLDPE for Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from Borstar FB2230 exhibits high dart impact combined with excellent yield and tensile strength and increased stiffness. Its toughness remains also in cold conditions. The film has high seal strength and hot tack force. Borstar FB2230 contains antioxidant.

Borstar BF2230 is well suited for a wide range of applications due to its unique balance of properties. The superior mechanical properties will improve the functionality of the films or allow for substantial material saving (down gauging) compared to conventional PEs. Some examples are: industrial liners, heavy duty sacks, compressed packs like diapers or insulation material, deep freeze packaging and agricultural applications.

Information provided by the Manufacturer.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Vapor Transmission, ISO 15106-2, 90% RH
  • Oxygen Transmission Rate, ASTM D3985, At 25°C/0% RH/1 bar
  • Thickness
  • Melt Flow, ISO 1133
  • Melt Flow, ISO 1133
  • High Load Melt Index, ISO 1133
  • Film Elongation at Break, MD, ISO 527-3
  • Film Elongation at Break, TD, ISO 527-3
  • Secant Modulus, MD, ISO 527-3, 0.05-1.05%
  • Secant Modulus, TD, ISO 527-3, 0.05-1.05%
  • Impact, ASTM 5748, Puncture Resistance, force (N)
  • Puncture Energy, ASTM 5748
  • Elmendorf Tear Strength, MD, ISO 6383/2
  • Elmendorf Tear Strength, TD, ISO 6383/2
  • Dart Drop, ISO 7765/1
  • Film Tensile Strength at Break, MD, ISO 527-3
  • Film Tensile Strength at Break, TD, ISO 527-3
  • Melting Point, ISO 11357/03
  • Vicat Softening Point, ISO 306, A (10N)
  • Haze, ASTM D1003
  • Gloss, ASTM D2457
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.