MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis Borstar® FB2230 LLDPE for Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from Borstar FB2230 exhibits high dart impact combined with excellent yield and tensile strength and increased stiffness. Its toughness remains also in cold conditions. The film has high seal strength and hot tack force. Borstar FB2230 contains antioxidant.

Borstar BF2230 is well suited for a wide range of applications due to its unique balance of properties. The superior mechanical properties will improve the functionality of the films or allow for substantial material saving (down gauging) compared to conventional PEs. Some examples are: industrial liners, heavy duty sacks, compressed packs like diapers or insulation material, deep freeze packaging and agricultural applications.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccISO 1183
Water Vapor Transmission 8.00 g/m²/day
@Temperature 38.0 °C
90% RH; ISO 15106-2
Oxygen Transmission Rate 5000 cc/m²/dayAt 25°C/0% RH/1 bar; ASTM D3985
Thickness 40.0 microns
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 0.90 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
High Load Melt Index 22 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 450 %ISO 527-3
Film Elongation at Break, TD 750 %ISO 527-3
Secant Modulus, MD 0.250 GPa0.05-1.05%; ISO 527-3
Secant Modulus, TD 0.300 GPa0.05-1.05%; ISO 527-3
Impact 65Puncture Resistance, force (N); ASTM 5748
Puncture Energy 5.00 JASTM 5748
Elmendorf Tear Strength, MD 0.0750 g/micronISO 6383/2
Elmendorf Tear Strength, TD 0.275 g/micronISO 6383/2
Dart Drop 7.50 g/micronISO 7765/1
Film Tensile Strength at Break, MD 55.0 MPaISO 527-3
Film Tensile Strength at Break, TD 45.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 124 °CISO 11357/03
Vicat Softening Point 101 °CA (10N); ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 70 %ASTM D1003
Gloss 10 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borstar® FB2310 LLDPE for Film
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
Dow ELITE™ 5100G Enhanced Polyethylene Resin
Dow ELITE™ 5500G Enhanced Polyethylene Resin
Dow DOWLEX™ 2047G Linear Low Density Polyethylene

PBOREA111 / 27418

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.