MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability and resistance to stress corrosion cracking.

Designated as UNS N08367, as is alloy AL6XN®1. The same ASTM, ASME and NACE specifications cover the alloys.

Alloy 25-6HN offers significantly improved strength and corrosion resistance in most environments over conventional austenitic stainless steels such as AISI 304 or 316L. Typical applications include welded tubes for heat exchangers for chemical processing and marine applications and for desalination systems, flue gas desulfurization equipment for coal-fired power plants, and reaction vessels for pharmaceutical production.

Information Provided by Special Metals Corporation

Key Words: UNS N08367; ASTM B 688, A240, B 691, B 564, B472, B 676, B 675, B 804, B 462, B 366
ASME SB688, SA240, SB691, SB564, SB472, SB676, SB675, SB804, SB462, SB366
Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B, Annealed Plate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, Annealed Plate
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield, Annealed Plate
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break, Annealed Plate
  • Elongation at Break
  • Magnetic Permeability, 200 Oersted
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Melting Point
  • Solidus
  • Liquidus
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe, Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Nitrogen, N
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Special Metals (includes the former Inco Alloys International Inc.)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.