MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability and resistance to stress corrosion cracking.

Designated as UNS N08367, as is alloy AL6XN®1. The same ASTM, ASME and NACE specifications cover the alloys.

Alloy 25-6HN offers significantly improved strength and corrosion resistance in most environments over conventional austenitic stainless steels such as AISI 304 or 316L. Typical applications include welded tubes for heat exchangers for chemical processing and marine applications and for desalination systems, flue gas desulfurization equipment for coal-fired power plants, and reaction vessels for pharmaceutical production.

Information Provided by Special Metals Corporation

Key Words: UNS N08367; ASTM B 688, A240, B 691, B 564, B472, B 676, B 675, B 804, B 462, B 366
ASME SB688, SA240, SB691, SB564, SB472, SB676, SB675, SB804, SB462, SB366
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.02 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 90Annealed Plate
Tensile Strength, Ultimate 80000 psi
@Temperature 538 °C
 84000 psi
@Temperature 427 °C
 86000 psi
@Temperature 260 °C
 87000 psi
@Temperature 316 °C
 89000 psi
@Temperature 204 °C
 93000 psi
@Temperature 149 °C
 107000 psi
@Temperature 21.1 °C
Annealed Plate
Tensile Strength, Yield 40.0 ksi
@Temperature 427 °C
 43.0 ksi
@Temperature 538 °C
 43.0 ksi
@Temperature 316 °C
 46.0 ksi
@Temperature 204 °C
 46.0 ksi
@Temperature 260 °C
 49.0 ksi
@Temperature 149 °C
 55.0 ksi
@Strain 2 %,
Temperature 21.1 °C
Annealed Plate
Elongation at Break 45 %
@Temperature 217 °C
 46 %
@Temperature 316 °C
 47 %
@Temperature 149 °C
 47 %
@Temperature 204 °C
 47 %
@Temperature 260 °C
 48 %
@Temperature 20.0 °C
Annealed Plate
 48 %
@Temperature 538 °C
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability 1.003
@Temperature 20.0 °C
200 Oersted
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.49 µin/in-°F
@Temperature 100 °C
 15.59 µm/m-°C
@Temperature 100 °C
 15.98 µm/m-°C
@Temperature 300 °C
 16.45 µm/m-°C
@Temperature 500 °C
 17.35 µm/m-°C
@Temperature 700 °C
Melting Point 2470 - 2560 °F
Solidus 2470 °F
Liquidus 2560 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.010 %
Chromium, Cr 20.6 %
Copper, Cu 0.25 %
Iron, Fe 47 %Balance
Manganese, Mn 0.40 %
Molybdenum, Mo 6.3 %
Nickel, Ni 24.3 %
Nitrogen, N 0.21 %
Phosphorus, P 0.020 %
Silicon, Si 0.30 %
Sulfur, S 0.0010 %
 
Descriptive Properties
Crevice Corrosion Temperature (°C)35per G48-D
 50in Green Death; Duration is 24 hours
Critical Pitting Temperature (°C)55Filler Metal: INCONEL 625; Welded Sample
 60Filler Metal: INCONEL 686; Welded Sample
 70in Green Death; Duration is 72 hours
 75per G48-C
Depth of Cut (in)0.15High Speed Steel Machining
 0.15Carbide Machining
Feed (in/rev)0.005High Speed Steel Drilling
 0.018High Speed Steel Machining
 0.018Carbide Machining
Pitting Resistance Equivalent Number48.3
Speed (SFPM)25High Speed Steel Machining
 25High Speed Steel Drilling
 350Carbide Machining

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCOLOY® 25-6MO Super Austenitic Stainless Steel (UNS N08926)
ATI Allvac® AL 6XN® UNS N08367 Specialty Steel
Alumina, alpha Al2O3, 99.5%
Special Metals INCOLOY® Alloy 925
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel

NINDA13 / 98904

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.