MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ExxonMobil Metallyte™ 15MM288 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. MM288 is designed for use as the center web of a triplex lamination. The treated surface offers good compatibility with adhesives and cohesives (cold seals).

Availability: Africa & Middle East, Asia Pacific and Europe

Key Features:

  • Excellent gas barrier
  • Excellent moisture barriers
  • Excellent light barrier
  • Enhances puncture resistance of the package
Features:
  • Flavor & Aroma Barrier
  • Gas Barrier
  • Grease Resistant
  • Light Barrier
  • Moisture Barrier
  • Oxygen Barrier
  • Puncture Resistant
  • Two Side Processable
Applications:
  • Crisps and Snacks
  • Dry Foods and Beverage Powders
  • Pet Food
Uses:
  • HFFS Flexible Packaging
  • Lidding – Flexible Packaging
  • Pouches – Flexible Packaging
  • Pre-made Bags – Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive and Inner Web Adhesive Lamination

Information provided by ExxonMobil

Vendors:
Available Properties
  • Water Vapor Transmission, ExxonMobil Method, 90% RH
  • Oxygen Transmission Rate, ExxonMobil Method, 0% RH
  • Thickness, ExxonMobil Method
  • Coating Weight, ExxonMobil Method
  • Modulus of Elasticity, ExxonMobil Method, MD
  • Modulus of Elasticity, ExxonMobil Method, TD
  • Shrinkage, MD, ExxonMobil Method
  • Shrinkage, TD, ExxonMobil Method
  • Optical Density, ExxonMobil Method
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.