Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. MM288 is designed for use as the center web of a triplex lamination. The treated surface offers good compatibility with adhesives and cohesives (cold seals). Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Excellent gas barrier
- Excellent moisture barriers
- Excellent light barrier
- Enhances puncture resistance of the package
Features: - Flavor & Aroma Barrier
- Gas Barrier
- Grease Resistant
- Light Barrier
- Moisture Barrier
- Oxygen Barrier
- Puncture Resistant
- Two Side Processable
Applications:- Crisps and Snacks
- Dry Foods and Beverage Powders
- Pet Food
Uses: - HFFS Flexible Packaging
- Lidding – Flexible Packaging
- Pouches – Flexible Packaging
- Pre-made Bags – Flexible Packaging
- VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive and Inner Web Adhesive LaminationInformation provided by ExxonMobil |