MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Metallyte™ 15MM288 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. MM288 is designed for use as the center web of a triplex lamination. The treated surface offers good compatibility with adhesives and cohesives (cold seals).

Availability: Africa & Middle East, Asia Pacific and Europe

Key Features:

  • Excellent gas barrier
  • Excellent moisture barriers
  • Excellent light barrier
  • Enhances puncture resistance of the package
Features:
  • Flavor & Aroma Barrier
  • Gas Barrier
  • Grease Resistant
  • Light Barrier
  • Moisture Barrier
  • Oxygen Barrier
  • Puncture Resistant
  • Two Side Processable
Applications:
  • Crisps and Snacks
  • Dry Foods and Beverage Powders
  • Pet Food
Uses:
  • HFFS Flexible Packaging
  • Lidding – Flexible Packaging
  • Pouches – Flexible Packaging
  • Pre-made Bags – Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive and Inner Web Adhesive Lamination

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Transmission 0.101 g/m²/day
@Temperature 38.0 °C
0.00650 g/100 in²/day
@Temperature 100 °F
90% RH; ExxonMobil Method
Oxygen Transmission Rate 15.1 cc/m²/day
@Temperature 23.0 °C
0.970 cc/100 in²/day
@Temperature 73.4 °F
0% RH; ExxonMobil Method
Thickness 15.0 microns0.590 milExxonMobil Method
Coating Weight 13.4 g/m²8.40 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 2.50 GPa363 ksiMD; ExxonMobil Method
 4.50 GPa653 ksiTD; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 3.0 %
@Temperature 135 °C,
Time 432 sec
3.0 %
@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 3.0 %
@Temperature 135 °C,
Time 432 sec
3.0 %
@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Optical Density 2.92.9ExxonMobil Method
 
Descriptive Properties
Yield51500 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Metallyte™ UHB 35MU842 OPP Film
ExxonMobil Metallyte™ UHB 35 MWHB OPP Film
ExxonMobil Metallyte™ 18MM383 OPP Film
ExxonMobil Bicor™ 21MB777 OPP Film
EMS-Grivory Grilon® FG 34 NL nat 6023 PA6

PEX99532 / 175768

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.