MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
SunChemical Gwent C2020509D1 Copper Ink  (discontinued **)
Categories: Fluid; Metal; Electronic/Magnetic Alloy; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: C2020509D1 is designed for BME End Terminations. The ink is designed for application using a Palomer dipping system. It can be used for Chipstar dippers, but the rheology needs of the customer have to be defined. It has excellent cosmetics and fires to a dense, smooth termination with high bond strength. It is designed to be used with standard Nickel/Tin Plating Systems.

This Ink has been made at a ready to use viscosity and should be gently stirred before use avoiding introduction of air bubbles.

Information provided by Gwent Electronic Materials Ltd.

Vendors:
Available Properties
  • Density
  • Solids Content
  • Viscosity, Haake VT550 cone and plate viscometer with the PK1.1°
  • Brookfield Viscosity, 10 rpm
  • Storage Temperature
  • Processing Temperature
  • Dry Time, with air flow
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Gwent Electronic Materials Ltd.

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.