MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Pyrotek ISOMAG® 175 Structural Insulation Board
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation provides a product with an outstanding combination of high compressive strength and low thermal conductivity. Incombustible, Isomag® 175 is totally free of asbestos and may be cut or machined with readily available tools.

Applications

  • Platen press insulation
  • Arc chutes
  • Resistor grids
  • Induction furnaces
  • Pot pads
  • Buss support insulation
  • Foundry bottom boards
  • Blow boards

Advantages

  • Low heat loss at higher temperatures
  • Low shrinkage at temperature use limit
  • High temperature rating
  • Asbestos and ceramic fiber free

Information provided by Pyrotek.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Water Absorption, with silicone treatment
  • Water Absorption
  • Open Porosity
  • Flexural Strength
  • Compressive Strength
  • Compressive Strength
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dielectric Breakdown
  • Dissipation Factor
  • Arc Resistance
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Maximum Service Temperature, Air, Continuous use
  • Maximum Service Temperature, Air
  • Flammability, UL94, V-0
  • Shrinkage, Linear
  • Shrinkage, Thickness
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Pyrotek, Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.