MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Pyrotek ISOMAG® 175 Structural Insulation Board
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation provides a product with an outstanding combination of high compressive strength and low thermal conductivity. Incombustible, Isomag® 175 is totally free of asbestos and may be cut or machined with readily available tools.

Applications

  • Platen press insulation
  • Arc chutes
  • Resistor grids
  • Induction furnaces
  • Pot pads
  • Buss support insulation
  • Foundry bottom boards
  • Blow boards

Advantages

  • Low heat loss at higher temperatures
  • Low shrinkage at temperature use limit
  • High temperature rating
  • Asbestos and ceramic fiber free

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.55 g/cc
Density 1.54 g/cc
Water Absorption <= 0.50 %with silicone treatment
 25 %
Open Porosity 44.1 %
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 27.6 MPa
Compressive Strength 37.9 MPa
 27.0 MPa
@Strain 5.0 %,
Temperature 500 °C
Izod Impact, Notched 0.900 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.90e+14 ohm-cm
Dielectric Constant 4.1
@Frequency 1000 Hz
Dielectric Strength 9.80 kV/mm
Dielectric Breakdown 28100 V
Dissipation Factor 0.050
Arc Resistance 292 sec
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.270 W/m-K
@Temperature 195 °C
 0.280 W/m-K
@Temperature 315 °C
 0.340 W/m-K
@Temperature 600 °C
Maximum Service Temperature, Air 1000 °CContinuous use
 1050 °C
Flammability, UL94 V-0V-0
Shrinkage 1.5 %
@Temperature 1000 °C
Linear
 4.3 %
@Temperature 1000 °C
Thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek ISOMAG® 70 Structural Insulation
Poraver 0.5-1 mm Expanded Glass
Pyrotek ISOMAG® 45 Thermal Insulation Board
Pyrotek NAD-250 Structural Insulation Board
Pyrotek B-3A REFRACTORY BOARD

CPYRO080 / 1818

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.