MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Architectural Bronze, UNS C38500
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass; Bronze

Material Notes: This is technically a brass alloy (copper plus zinc) but is known as architectural bronze. Fair to excellent corrosion resistance. Excellent machinability and hot workability. Fabricated by hot forging and pressing, forming, bending and machining.

Applications: architectural extrusion, store fronts, thresholds, trim, butts, hinges, lock bodies and forgings.

Available as rod, shapes.

Key Words: British Free Machining Brass, BS 2874 CZ121, ISO CuZn39Pb3
Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B, M30 temper
  • Tensile Strength, Ultimate, M30 temper
  • Tensile Strength, Yield, M30 temper
  • Elongation at Break, in 50 mm, M30 temper
  • Modulus of Elasticity
  • Poissons Ratio, Calculated
  • Machinability, UNS C36000 (free-cutting brass) = 100%
  • Shear Modulus
  • Shear Strength, M30 temper
  • Electrical Resistivity
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Annealing Temperature
  • Hot-Working Temperature
  • Copper, Cu
  • Iron, Fe
  • Lead, Pb
  • Other, total
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.