MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Architectural Bronze, UNS C38500
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass; Bronze

Material Notes: This is technically a brass alloy (copper plus zinc) but is known as architectural bronze. Fair to excellent corrosion resistance. Excellent machinability and hot workability. Fabricated by hot forging and pressing, forming, bending and machining.

Applications: architectural extrusion, store fronts, thresholds, trim, butts, hinges, lock bodies and forgings.

Available as rod, shapes.

Key Words: British Free Machining Brass, BS 2874 CZ121, ISO CuZn39Pb3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.47 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 65M30 temper
Tensile Strength, Ultimate 415 MPaM30 temper
Tensile Strength, Yield 140 MPa
@Strain 0.5 %
M30 temper
Elongation at Break 30 %in 50 mm, M30 temper
Modulus of Elasticity 97.0 GPa
Poissons Ratio 0.31Calculated
Machinability 90 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 37.0 GPa
Shear Strength 240 MPaM30 temper
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000620 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.9 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 123 W/m-K
@Temperature 20.0 °C
Melting Point 875 - 890 °C
Solidus 875 °C
Liquidus 890 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 600 °C
Hot-Working Temperature 625 - 725 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 55 - 60 %
Iron, Fe <= 0.35 %
Lead, Pb 2.0 - 3.8 %
Other, total <= 0.50 %
Zinc, Zn 40 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Free-Cutting Brass, UNS C36000
Architectural Bronze, UNS C38000
Forging Brass, UNS C37700
Chicago Extruded Metals UNS C38500 Copper-Zinc-Lead Alloy
Mueller Alloy 3850 Architectural Brass (UNS C38500)

MC38500b1 / 11254

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.