MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Ensinger TECACOMP LCP LDS black 1049426 Liquid crystal polymer
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Unfilled

Material Notes:
  • developed for the LPKF-LDSĀ® process
  • very low melt viscosity
  • very good chemical resistance
  • inherent flame retardant
  • good heat deflection temperature
  • low moisture absorption
Target Industries:
  • automotive industry
  • electrical engineering
  • LED lighting technology
  • mechanical engineering

Information provided by Ensinger Inc.

Vendors:
Available Properties
  • Density
  • Water Absorption at Saturation, DIN EN ISO 62, 50 % relative humidity up to saturation
  • Linear Mold Shrinkage, Flow, DIN EN ISO 294-4
  • Linear Mold Shrinkage, Transverse, DIN EN ISO 294-4
  • Tensile Strength, DIN EN ISO 527-1
  • Elongation at Break, DIN EN ISO 527-1
  • Modulus of Elasticity, DIN EN ISO 527-1
  • Charpy Impact Unnotched, DIN EN ISO 179-1eU
  • Volume Resistivity, DIN EN 61340-2-3
  • Surface Resistance, DIN EN 61340-2-3
  • Dielectric Constant
  • Dissipation Factor
  • Comparative Tracking Index, DIN EN 60112
  • CTE, linear, Parallel to Flow, DIN EN ISO 11359-1;2
  • CTE, linear, Parallel to Flow, DIN EN ISO 11359-1;2
  • CTE, linear, Parallel to Flow, DIN EN ISO 11359-1;2
  • CTE, linear, Parallel to Flow, DIN EN ISO 11359-1;2
  • CTE, linear, Transverse to Flow, DIN EN ISO 11359-1;2
  • CTE, linear, Transverse to Flow, DIN EN ISO 11359-1;2
  • CTE, linear, Transverse to Flow, DIN EN ISO 11359-1;2
  • CTE, linear, Transverse to Flow, DIN EN ISO 11359-1;2
  • Thermal Conductivity, ISO 22007-4:2008, through-plane
  • Thermal Conductivity, ISO 22007-4:2008, in-plane
  • Melting Point, DIN 53765
  • Maximum Service Temperature, Air, long term
  • Maximum Service Temperature, Air, short term
  • Deflection Temperature at 1.8 MPa (264 psi), ISO-R 75 Method A
  • Flammability, UL94, DIN IEC 60695-11-10
  • Processing Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.