MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Protective Coating PC-Rot Terminator® Epoxy Wood Consolidant
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: PC-Rot Terminator® is designed to strengthen decayed or rotted wood. The mixture is a low viscosity liquid that penetrates porous surfaces filling and sealing voids with an epoxy that cures to a hard but durable component. Rot Terminator® combines an extended open time and low viscosity without solvents. The Rot Terminator® is useful for replacement of missing wood fibers or wood resin. It fills the void in the wood with an elastomer that has strength greater than wood. Typical wood resin has low tensile and compressive properties when compared to cured epoxy polymer in wood. The epoxy act as a binder that glues the wood fibers together. The wood fibers become much stronger in combination with the epoxy elastomer. It is mixed one part hardener to two parts resin.

Key Words: PC Epoxy
Vendors:
Available Properties
  • Viscosity, Hardener
  • Viscosity, Mixed
  • Viscosity, Resin
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Tensile Modulus
  • Flexural Strength
  • Flexural Modulus
  • Compressive Yield Strength
  • Compressive Modulus
  • Flash Point, Hardener, closed cup
  • Flash Point, Resin, closed cup
  • Gardner Color Number, Resin
  • Gardner Color Number, Mix
  • Gardner Color Number, Hardener
  • Cure Time
  • Cure Time
  • Cure Time, Thin Film Set
  • Cure Time, Maximum Cure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Protective Coating Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.